HS-1013C-P Unsaturated Polyester Resin for Flame-retardant Lighting Panels

HS-1013C-P is an unsaturated polyester resin specially used for the production of flame-retardant lighting panels, which has good light transmittance, mechanical strength, flame-retardant properties, good weathering and yellowing resistance. It is suitable for mechanism/hand lay-up process.

Availability:
  • HS-1013C-P

  • Huake

Product Description

HS-1013C-P Unsaturated Polyester Resin 

Principal Properties & Application

HS-1013C-P is an unsaturated polyester resin specially used for the production of flame-retardant lighting panels, which has good light transmittance, mechanical strength, flame-retardant properties, good weathering and yellowing resistance. It is suitable for mechanism/hand lay-up process.

 

Specifications of liquid resin

Item

Unit

Standard Requirements

Test Method

Appearance

――

Purple-red transparent liquid

GB/T8237.6.1.1

Viscosity

25℃, CP

180-260

GB/T7193.4.1

SPI-GT

min

0.5 -1.5

GB/T 7193.4.4

SPI-CT

min

1.8 - 3.0

GB/T 7193.4.4

SPI-PET

175-210

GB/T 7193.4.4

To test the SPI curing characteristics, the curing system is: Curing agent M-50: 1.2 %

 

Physical properties of Casting(for reference only)

Item

Unit

Test Value

Test Method

Tensile Strength

MPa

55

GB/T 2568

Elongation at Break

%

3.8

GB/T 2568

Bending Strength

MPa

107

GB/T 2570

Heat Distortion Temperature

63

GB/T 1634

Oxygen index

%

26

GB/T 3854

 

Note:

1) Pouring system according to GB/T 8237-2005, curing system: curing agent M-50: 2%;

2) Curing system after casting is: room temperature (24 h) + 60℃ (3 h) + 100℃ (2 h).

 

Caution:

1, Transportation should be in accordance with the State Council “Regulations on the Safe Management of Dangerous Chemicals”, Chapter V of the safety regulations on the transportation of chemical hazardous substances. The product should be stored in a cool place under 25℃, avoiding fire, isolating heat source, and sealed to prevent moisture intrusion and volatilization of the monomer. the shelf life of the product is 3 months under 25℃.


Previous: 
Next: 

Subscribe To Our Newsletter

Leave your email address to get the latest product information from our company at any time.
Changzhou Huake polymer Co., Ltd. specializes in the R & D, production and sales of a series of products such as unsaturated polyester resin, vinyl resin and so on.

QUICK LINKS

PRODUCTS

GET IN TOUCH

  +86-19802502976
 sales@huakepolymers.com
 No.602, North Yulong Road,
Xinbei District, Changzhou City,
Jiangsu Province, China.
Copyright © 2024 Changzhou Huake polymer Co., Ltd. All Rights Reserved.  Supported by leadong.com     Sitemap